Home/Standards/ASTM C273 / ASTM C393
ASTM C273 / ASTM C393ISO: ISO 1922 / ISO 844Sandwich Composite Cores

Core Shear & Sandwich Panel Mechanics

Standard Test Method for Shear Properties of Sandwich Core Materials & Core Shear in Flatwise Flexure

Request Custom Testing RFQ
Methodology & Apparatus

Testing Protocol

In ASTM C273 (block shear), the core specimen is bonded between two parallel heavy steel loading plates and pulled in tension or compression along the plane of the facing. In ASTM C393 (beam flexure), a sandwich beam (skin facings + core) is supported on two cylindrical supports and loaded at quarter-points to produce pure core shear failure without facing rupture.

Specimen Configuration

Geometry & Dimensions

ASTM C273: length 12 times thickness (e.g., 200 x 50 x 20 mm). ASTM C393: standard sandwich beam length 200 mm, width 75 mm, nominal core thickness 12.7 to 25.4 mm with 1.5 mm composite skins.

Loading Speed: Test speed produces failure within 3 to 6 minutes (typically 0.5 to 1.5 mm/min).
Naval & Aero Utility

Engineering Importance

Indispensable for hull bottom sandwich core sizing (Divinycell H80, Corecell M80, Rohacell, Baltek balsa). Prevents catastrophic core shear fracture and skin-to-core debonding under heavy sea slamming.

Industry Benchmark Ranges: ASTM C273 / ASTM C393

Normalized baseline values across major North American composite resin and core chemistries.

Standardized at 23°C / 50% RH
Material Chemistry / FamilyTypical Benchmark RangeMarine & Industrial Application Context
End-Grain Balsa Core (Baltek SB.100 - 150 kg/m³)2.8 – 3.8 MPa (406 – 551 psi)Highest shear strength per density; standard for commercial workboats and wind turbine blades.
Structural SAN Foam Core (Corecell M80 - 80 kg/m³)1.2 – 1.6 MPa (174 – 232 psi)Exceptional fatigue life and dynamic slam resistance for high-speed ocean racing hulls.
Cross-Linked PVC Foam (Divinycell H80 - 80 kg/m³)1.0 – 1.3 MPa (145 – 188 psi)Global industry workhorse core for yacht hulls, decks, and marine superstructures.
Aerospace PMI Foam Core (Rohacell 71 IG-F)1.3 – 1.7 MPa (188 – 246 psi)High-temperature resistance for 180°C autoclave prepreg curing with zero outgassing.

Verified Materials in US Catalog (30 SKU)

Parametric test results pulled live from the CompositeMatrix™ PostgreSQL material graph.

Material NameManufacturerCategoryTested ParameterHazmat ClassActions
3A Composites Airex C70.75 Cross-Linked PVC Sandwich Core3A CompositesStructural Sandwich Core80 kg/m³Non-Regulated Solid PolymerSpecs & BOM →
3A Composites Airex T92.100 Structural PET Foam Core3A CompositesRecyclable PET Foam Core105 kg/m³Non-Regulated Solid PolymerSpecs & BOM →
3A Composites Baltek SB.100 Structural End-Grain Balsa Core3A CompositesStructural Sandwich Core155 kg/m³Non-Regulated Solid PolymerSpecs & BOM →
3M Scotch-Weld DP420 Toughened Two-Part Epoxy Adhesive3M Industrial AdhesivesStructural Epoxy Adhesive1120 kg/m³Class 8 CorrosiveSpecs & BOM →
3M Scotch-Weld DP460 High-Peel Carbon Bonding Epoxy3M Industrial AdhesivesStructural Epoxy Adhesive1120 kg/m³Class 8 CorrosiveSpecs & BOM →
3M Scotch-Weld DP8407NS Toughened Acrylic Metal/Composite Adhesive3M Industrial AdhesivesToughened Acrylic Structural Adhesive1140 kg/m³Class 3 Flammable LiquidSpecs & BOM →
3M Scotch-Weld EC-2216 B/A Gray Flexible Aerospace Epoxy Adhesive3M Industrial AdhesivesAerospace Flexible Epoxy Adhesive1140 kg/m³Class 9 Environmentally HazardousSpecs & BOM →
Advantex® Corrosion-Resistant Direct RovingOwens CorningE-CR Fiberglass1120 kg/m³Non-Hazmat Palletized FreightSpecs & BOM →
AGY S-2 Glass High-Strength Ballistic & Aerospace RovingAGY Holding Corp (Aiken, SC)E-Glass & Aramid Multiaxial2560 kg/m³Non-Regulated Industrial FiberSpecs & BOM →
Airtech Airweave N10 Non-Woven Polyester Breather & BleederAirtech Advanced MaterialsAutoclave Breather Felt1120 kg/m³Non-Regulated Industrial ConsumableSpecs & BOM →
Airtech AT-200Y Economical Ambient Infusion Sealant TapeAirtech Advanced MaterialsInfusion Tacky Tape1120 kg/m³Non-Regulated Industrial ConsumableSpecs & BOM →
Airtech Dahlpac MC79 Combined Peel Ply + Release Film + Flow MeshAirtech Advanced Materials3-in-1 Infusion Consumable Pack1120 kg/m³Non-Regulated Industrial ConsumableSpecs & BOM →
Airtech Econostitch 85 gsm Nylon Pin-Striped Peel PlyAirtech Advanced MaterialsRelease Peel Ply Fabric1120 kg/m³Non-Regulated Industrial ConsumableSpecs & BOM →
Airtech Greenflow 75 High-Speed Extruded Resin Flow MediaAirtech Advanced MaterialsHDPE Infusion Flow Mesh1120 kg/m³Non-Regulated Industrial ConsumableSpecs & BOM →
Airtech GS-213-3 High-Tack Vacuum Bag Sealant Tape (Tacky Tape)Airtech Advanced MaterialsButyl Vacuum Sealant Tape1120 kg/m³Non-Regulated Industrial ConsumableSpecs & BOM →
Airtech Ipplon KM1300 Soft-Drape Marine Infusion Bagging FilmAirtech Advanced MaterialsCo-Extruded Nylon Bagging Film1120 kg/m³Non-Regulated Industrial ConsumableSpecs & BOM →
Airtech Omega Flow Line Silicone Resin Infusion ChannelAirtech Advanced MaterialsReusable Silicone Feed Channel1120 kg/m³Non-Regulated Industrial ConsumableSpecs & BOM →
Airtech Release Ease 234 TFP PTFE-Coated Fiberglass Peel PlyAirtech Advanced MaterialsPTFE Coated Peel Ply1120 kg/m³Non-Regulated Industrial ConsumableSpecs & BOM →
Airtech Resinflow 90 Heavy-Duty Hull Infusion Distribution MeshAirtech Advanced MaterialsInfusion Distribution Mesh1120 kg/m³Non-Regulated Industrial ConsumableSpecs & BOM →
Airtech Toolfusion 1A / 1B High-Tg Epoxy Infusion Tooling ResinAirtech Advanced MaterialsHigh-Tg Tooling Infusion Epoxy1150 kg/m³Class 9 Environmentally HazardousSpecs & BOM →

Technical FAQs on ASTM C273 / ASTM C393

What causes core shear failure in boat hulls?

When a hull slams against waves at high speed, the bottom panel experiences intense hydrodynamic transverse pressure. If the core's shear strength (ASTM C273/C393) is exceeded, the core ruptures in diagonal 45-degree shear cracks, leading to rapid skin debonding and water ingress.

How does resin priming affect core shear performance?

Pre-priming foam core surface cells with resin before infusion prevents 'resin-starved' bonding interfaces. A fully filled surface cell structure ensures skin-to-core peel strength exceeds the core's own cohesive shear strength.