Standard Test Method for Indentation Hardness of Rigid Plastics by Means of a Barcol Impressor
A spring-loaded hardened steel truncated cone indenter (26° angle with flat tip of 0.157 mm diameter) is pressed perpendicular to the smooth specimen surface by hand with uniform firm pressure until dial indicator peaks. The hardness value is read directly on the 0–100 dial scale. Standard procedure specifies taking at least 10 independent readings on clean composite surfaces.
Specimens must have a minimum thickness of 1.5 mm (0.06 in) and be supported on a firm rigid backing to prevent deflection. Surface must be free of wax, dust, and peel-ply texture.
Indispensable shop-floor QC gate: dictates the exact moment a yacht hull or windmill blade can safely be demolded without permanent hull warpage. Also confirms that gelcoat has cured beyond air inhibition.
Normalized baseline values across major North American composite resin and core chemistries.
| Material Chemistry / Family | Typical Benchmark Range | Marine & Industrial Application Context |
|---|---|---|
| Fully Cured Marine Vinyl Ester (Derakane / CoREZYN) | 35 – 45 Barcol | Demold standard is typically >= 30 Barcol; full mechanical properties reached at 35–42. |
| Rigid Tooling Gelcoats & Vinyl Ester Tooling Resin | 42 – 52 Barcol | High surface hardness prevents mold scratching during repeated demolding cycles. |
| Marine Isophthalic Polyesters | 38 – 48 Barcol | Standard hull resin cure verification threshold is >= 35 Barcol. |
| Under-Cured or Air-Inhibited Laminate | < 25 Barcol | Indicates insufficient catalyst, cold shop temperature (<18°C), or styrene loss. Demolding prohibited. |
Parametric test results pulled live from the CompositeMatrix™ PostgreSQL material graph.
| Material Name | Manufacturer | Category | Tested Parameter | Hazmat Class | Actions |
|---|---|---|---|---|---|
| Airtech Toolfusion 1A / 1B High-Tg Epoxy Infusion Tooling Resin | Airtech Advanced Materials | High-Tg Tooling Infusion Epoxy | 44 Barcol | Class 9 Environmentally Hazardous | Specs & BOM → |
| PRO-SET TLG-125 / TLG-229 High-Temperature Tooling Laminating Epoxy | Gougeon Brothers (PRO-SET) | High-Tg Tooling Infusion Epoxy | 44 Barcol | Class 9 Environmentally Hazardous | Specs & BOM → |
| Araldite® LY 1564 / Aradur® 22962 | Huntsman Advanced | Epoxy System | 42 Barcol | US DOT Class 8 / 9 (Corrosive Polyamine Hardener) | Specs & BOM → |
| Gurit Ampreg 31 DNV-GL Certified Laminating Epoxy | Gurit | Infusion Epoxy | 42 Barcol | Class 9 Environmentally Hazardous | Specs & BOM → |
| Gurit Ampreg 36 High-Tg Aerospace & Marine Epoxy | Gurit | Infusion Epoxy | 42 Barcol | Class 9 Environmentally Hazardous | Specs & BOM → |
| Gurit Prime 27 Ultra-Low Viscosity Infusion Epoxy | Gurit | Infusion Epoxy | 42 Barcol | Class 9 Environmentally Hazardous | Specs & BOM → |
| Gurit Prime 37 Infusion Epoxy System | Gurit | Infusion Epoxy | 42 Barcol | Class 9 Environmentally Hazardous | Specs & BOM → |
| Hexion EPON Resin 828 Unmodified Bisphenol-A Epoxy | Hexion | Infusion Epoxy | 42 Barcol | Class 9 Environmentally Hazardous | Specs & BOM → |
| Hexion EPON Resin 862 Low-Viscosity Bisphenol-F Epoxy | Hexion | Infusion Epoxy | 42 Barcol | Class 9 Environmentally Hazardous | Specs & BOM → |
| HK Research MaxGuard NP White Marine ISO/NPG Gelcoat | HK Research Corp | ISO/NPG Marine Gelcoat | 42 Barcol | Class 3 Flammable Liquid | Specs & BOM → |
| Huntsman Araldite LY 1564 SP Infusion Epoxy Resin | Huntsman Advanced Materials | Infusion Epoxy | 42 Barcol | Class 9 Environmentally Hazardous | Specs & BOM → |
| Huntsman Araldite LY 5052 Cold-Cure Aerospace Epoxy | Huntsman Advanced Materials | Infusion Epoxy | 42 Barcol | Class 9 Environmentally Hazardous | Specs & BOM → |
| Huntsman Araldite MY 721 Tetrafunctional Aerospace Epoxy | Huntsman Advanced Materials | Infusion Epoxy | 42 Barcol | Class 9 Environmentally Hazardous | Specs & BOM → |
| PRO-SET HTP-124 High-Temperature Tooling Epoxy | Gougeon Brothers (PRO-SET) | Infusion Epoxy | 42 Barcol | Class 9 Environmentally Hazardous | Specs & BOM → |
| PRO-SET INF-114 High-Tg Carbon Infusion Epoxy | Gougeon Brothers (PRO-SET) | Infusion Epoxy | 42 Barcol | Class 9 Environmentally Hazardous | Specs & BOM → |
| PRO-SET LAM-125 Medium Viscosity Laminating Epoxy | Gougeon Brothers (PRO-SET) | Infusion Epoxy | 42 Barcol | Class 9 Environmentally Hazardous | Specs & BOM → |
| PRO-SET LAM-135 Low-Viscosity Wet-Out Epoxy | Gougeon Brothers (PRO-SET) | Infusion Epoxy | 42 Barcol | Class 9 Environmentally Hazardous | Specs & BOM → |
| Sicomin SR 5550 Lloyd's Approved Structural Epoxy | Sicomin North America | Infusion Epoxy | 42 Barcol | Class 9 Environmentally Hazardous | Specs & BOM → |
| Sicomin SR 8100 Low-Toxicity Marine Infusion Epoxy | Sicomin North America | Infusion Epoxy | 42 Barcol | Class 9 Environmentally Hazardous | Specs & BOM → |
| System Three SilverTip Marine Laminating Epoxy | System Three Resins | Infusion Epoxy | 42 Barcol | Class 9 Environmentally Hazardous | Specs & BOM → |
Most naval architects and resin manufacturers (AOC, Polynt, Ashland) specify a minimum Barcol hardness of 30 to 35 (Model 934-1) before pulling a large hull from the female mold. Demolding below 28 Barcol risks hull distortion, print-through, and permanent sagging on trailer bunks.
Yes, but Model 934-1 is calibrated for rigid thermosets with Barcol > 25. For softer room-temperature epoxies or polyurethane tooling blocks, Shore D hardness (ASTM D2240) is frequently used as a complementary measurement.