Standard Test Method for Tensile Properties of Plastics & Advanced Polymer Matrix Composites
Specimens are gripped in universal testing machine (UTM) wedge grips with an optical or mechanical extensometer attached to the gauge length. Load is applied at a constant crosshead speed (5 mm/min / 0.2 in/min for rigid thermosets) until fracture, recording stress-strain curves, tensile yield, ultimate tensile strength (UTS), tensile modulus of elasticity (Young's modulus), and elongation at break (%).
Type I Dogbone (overall length 165 mm / 6.5 in, narrow gauge width 13 mm / 0.5 in, thickness 3.2 mm / 0.125 in). For D3039: straight rectangular coupon (250 x 25 mm) with bonded beveled composite or aluminum end tabs.
Critical for marine hull skin laminate sizing, wind turbine spar cap design, and pressure vessels under internal hydrostatic or tensile stress. Ensures laminates withstand cyclic hydrodynamic wave slapping without micro-cracking.
Normalized baseline values across major North American composite resin and core chemistries.
| Material Chemistry / Family | Typical Benchmark Range | Marine & Industrial Application Context |
|---|---|---|
| Marine Vinyl Ester Resins (Neat) | 75 – 86 MPa (10,800 – 12,500 psi) | High tensile elongation (4.0–6.0%) provides exceptional micro-cracking resistance. |
| Structural Epoxy Systems (Neat) | 68 – 92 MPa (9,800 – 13,300 psi) | Superior inter-laminar shear and fatigue endurance in aerospace and racing yachts. |
| Isophthalic Marine Polyesters (Neat) | 52 – 72 MPa (7,500 – 10,400 psi) | Standard marine hull structural resin; elongation typically 2.0–3.5%. |
| Carbon Fiber / Epoxy Laminates (0° UD) | 1,500 – 2,600 MPa (217,000 – 377,000 psi) | Primary structural spar caps, aerospace stringers, and hydrofoil foils. |
| E-Glass 1708 Biaxial Infused Laminates (0/90) | 280 – 420 MPa (40,600 – 60,900 psi) | Primary boat hull shell and stringer reinforcement in modern infusion boatbuilding. |
Parametric test results pulled live from the CompositeMatrix™ PostgreSQL material graph.
| Material Name | Manufacturer | Category | Tested Parameter | Hazmat Class | Actions |
|---|---|---|---|---|---|
| Toray Torayca T1000G Ultra-High Strength Aerospace Carbon | Toray Composite Materials America | Carbon Fiber & Prepreg | 6370 MPa (923,892 psi) | Non-Regulated Industrial Fiber | Specs & BOM → |
| Teijin Tenax IMS65 24K Intermediate Modulus Carbon | Teijin Carbon America | Carbon Fiber & Prepreg | 6000 MPa (870,228 psi) | Non-Regulated Industrial Fiber | Specs & BOM → |
| Toray Torayca T800S Intermediate Modulus Carbon Fiber | Toray Composite Materials America | Intermediate Modulus Carbon | 5880 MPa (852,823 psi) | Non-Regulated Industrial Fiber | Specs & BOM → |
| Hexcel HexTow IM7 12K Intermediate Modulus Carbon Fiber | Hexcel Corporation | Carbon Fiber & Prepreg | 5650 MPa (819,465 psi) | Non-Regulated Industrial Fiber | Specs & BOM → |
| Mitsubishi Pyrofil TR50S 15K High-Strength Industrial Carbon | Mitsubishi Chemical Carbon Fiber US | Carbon Fiber & Prepreg | 4900 MPa (710,686 psi) | Non-Regulated Industrial Fiber | Specs & BOM → |
| Hexcel HexTow AS4 12K Aerospace Qualified Carbon Fiber | Hexcel Corporation | Carbon Fiber & Prepreg | 4410 MPa (639,618 psi) | Non-Regulated Industrial Fiber | Specs & BOM → |
| Mitsubishi Pyrofil TR30S 3K 200 gsm 2x2 Twill Carbon Fiber Fabric | Mitsubishi Chemical Carbon Fiber US | 3K Woven Carbon Fabric | 4410 MPa (639,618 psi) | Non-Regulated Reinforcement (EAR 1C010 / EAR99) | Specs & BOM → |
| Toray Torayca M40J High-Modulus Pitch/PAN Carbon Fiber | Toray Composite Materials America | Carbon Fiber & Prepreg | 4400 MPa (638,167 psi) | Non-Regulated Industrial Fiber | Specs & BOM → |
| Chomarat C-Ply BX600 Spread-Tow Biaxial (+/-45) Carbon | Chomarat North America | Carbon Fiber & Prepreg | 4250 MPa (616,412 psi) | Non-Regulated Industrial Fiber | Specs & BOM → |
| Hexcel HexForce G0926 6K 5HS Satin Carbon Fabric (370 gsm) | Hexcel Corporation | Carbon Fiber & Prepreg | 4120 MPa (597,557 psi) | Non-Regulated Industrial Fiber | Specs & BOM → |
| Chomarat C-Weave 200T 3K 2x2 Twill Carbon Fabric | Chomarat North America | Carbon Fiber & Prepreg | 3980 MPa (577,251 psi) | Non-Regulated Industrial Fiber | Specs & BOM → |
| Hexcel HexForce 3733 3K Plain Weave Carbon Fabric (197 gsm) | Hexcel Corporation | Carbon Fiber & Prepreg | 3850 MPa (558,396 psi) | Non-Regulated Industrial Fiber | Specs & BOM → |
| HexForce® 282 3K Plain Weave Carbon | Hexcel Corp | Carbon Fiber | 3792.1 MPa (550,000 psi) | Non-Hazmat Standard Freight | Specs & BOM → |
| Toray Torayca T300 3K Standard Modulus Carbon Tow | Toray Composite Materials America | Carbon Fiber & Prepreg | 3530 MPa (511,984 psi) | Non-Regulated Industrial Fiber | Specs & BOM → |
| Advantex® Corrosion-Resistant Direct Roving | Owens Corning | E-CR Fiberglass | 3378.4 MPa (490,000 psi) | Non-Hazmat Palletized Freight | Specs & BOM → |
| Teijin Twaron CT 736 Par-Aramid Ballistic & Marine Impact Fabric | Teijin Aramid USA | Para-Aramid Ballistic Fabric | 3200 MPa (464,122 psi) | Non-Regulated Reinforcement (EAR 1C010 / EAR99) | Specs & BOM → |
| Vectorply® E-BXM 1708 Biaxial E-Glass | Vectorply Corp | Marine Fiberglass | 3102.6 MPa (450,000 psi) | Non-Hazmat Standard Freight | Specs & BOM → |
| Hexcel HexPly M21 Primary Structure Aerospace Carbon Prepreg | Hexcel Corporation | Carbon Fiber & Prepreg | 2850 MPa (413,358 psi) | Non-Regulated Industrial Fiber | Specs & BOM → |
| Hexcel HexPly 8552 / IM7 180°C Autoclave Primary Aerospace Prepreg | Hexcel Corporation | Aerospace Toughened Epoxy Prepreg (EAR 1C010) | 2720 MPa (394,503 psi) | Refrigerated Non-Hazmat (Dry Ice UN1845 if Air) • EAR Screening | Specs & BOM → |
| Hexcel HexPly 8552 / IM7 Toughened Autoclave Epoxy Prepreg | Hexcel Corporation | Carbon Fiber & Prepreg | 2720 MPa (394,503 psi) | Non-Regulated Industrial Fiber | Specs & BOM → |
ASTM D638 is designed for neat (unreinforced) plastics and short-fiber compounds using dumbbell dogbone specimens. ASTM D3039 is specifically engineered for high-strength continuous fiber reinforced polymer composites (CFRP/GFRP) using straight rectangular coupons with bonded end-tabs to prevent grip-induced crushing.
Marine hulls undergo dynamic hydrodynamic slamming impacts. Resins with tensile elongation below 2% develop microscopic matrix micro-cracks beneath gelcoats, leading to osmotic blistering and delamination. Vinyl esters with 4-6% elongation absorb impact energy elastically.
Post-curing neat vinyl esters and structural epoxies at elevated temperatures (e.g., 60°C–80°C for 4–8 hours) elevates cross-link density from ~80% to >98%, increasing tensile strength by 15–25% and tensile modulus by 10–20%.